spun fiber
rotating glass preform during fiber drawing process produces a waveguide with unique properties: all fiber non-uniformities are averaged along all possible directions,effectively cancelling out total fiber birefringence. with total (but not local)birefringence close to zero, we obtain a fiber that will hold circular polarization (even when bent or twisted). unlike conventional pm fibers that can hold only linearly polarized light, or annealed fiber that requires special handling, this low-birefringence fiber preserves both linear and circular polarization and can relay it with minimum error over large distances.
highly-birefringent preforms with incorporated stress produce spun fibers that can withstand significant bending and twisting and hold polarization over large number of coils with reasonable accuracy (without costly annealing process). polarization accuracy in this case depends on local (instant) birefringence that introduces a small constant error, independent of fiber length.
elliptical core fiber
our elliptical-core pme1300-10 fiber provides high polarization extinction and insensitivity to bending and twisting stress. unlike conventional pm fibers, birefringence of the elliptical-core waveguide has low thermal dependence (10 times lower than panda).
due to core geometry the splice losses to a conventional circular-core fiber (smf, panda or bow-tie) are asymmetrical - 0.5 db for circular-toelliptical coupling and 2.5 db for elliptical-to-circular arrangement.
features
- high extinction ratio
- reduced coupling loss
- low temperature dependence
applications
- fiber-optic gyros
- optical current sensors
- fiber amplifiers
specifications
lb650
lb1060
lb1300
lb1300rc
pme1300-10
operating wavelength
600 - 900 nm
900 - 1100 nm
1300 - 1600 nm
1300 - 1600 nm
1300 - 1600 nm
cut-off wavelength
< 580 nm
< 915 nm
< 1280 nm
< 1280 nm
< 1280 nm
beatlength
4 mm
7 mm
13 mm
13 mm
9 mm
spin period
3 mm
3 mm
3 mm
3 mm
—
attenuation
6 db/km
6 db/km
4 db/km
5 db/km
8 db/km
mode field dimensions
6 um
8 um
9 um
9 um
13 x 8 um
cladding diameter
125 um
125 um
125 um
80 um
125 um
coating diameter
250 um
250 um
250 um
200 um
250 um
core-clad concentricity
< 0.5 um
< 0.5 um
< 0.5 um
< 0.5 um
< 0.5 um
cladding offset
< 5 um
< 5 um
< 5 um
< 5 um
< 5 um
coating material
acrylate
acrylate
acrylate
acrylate
acrylate
proof test
100 kpsi
100 kpsi
100 kpsi
100 kpsi
100 kpsi
bending radius
> 20 mm
> 20 mm
> 20 mm
> 12 mm
> 20 mm